Gwifren Syth Titaniwm
Enw: gwifren syth titaniwm
Dimensiwn: Dia (0. 8-6. 0) XL (10-6000) mm
Deunydd: Ti-6AL-4V Ti-0.2Pd Ti-3AL-2.5V TI-0.2Pd ELI Ti-0.3Mo-0.8Ni Ti-6Al-4V ELI
Dull Prosesu: Tynnu poeth / Tynnu oer
Arwyneb gorffenedig: Sgleinio / Piclo
Cyflwr: Annealing / Oer wedi'i dynnu
ASTM B.863Cyfansoddiad Cemegol gwifren titaniwm | |||||||||||
Gradd | N | C | H | Fe | O | Al | V | Pa | Mo. | Ni | Ti |
GR 1 | 0.03 | 0.08 | 0.015 | 0.20 | 0.18 | / | / | / | / | / | |
GR 2 | 0.03 | 0.08 | 0.015 | 0.30 | 0.25 | / | / | / | / | / | |
GR 5 | 0.05 | 0.08 | 0.015 | 0.40 | 0.20 | 5.5~6.75 | 3.5~4.5 | / | / | / | |
GR 7 | 0.03 | 0.08 | 0.015 | 0.30 | 0.25 | / | / | 0.12~0.25 | / | / | |
GR 9 | 0.03 | 0.08 | 0.015 | 0.25 | 0.15 | 2.5~3.5 | 2.0~3.0 | / | / | / | |
GR 12 | 0.03 | 0.08 | 0.125 | 0.30 | 0.25 | / | / | / | 0.2~0.4 | 0.6~0.9 | bal |
Mae titaniwm yn fetel pontio arian-gwyn, gyda phwysau ysgafn, cryfder uchel, ymwrthedd cyrydiad da a nodweddion eraill, mae ei briodweddau cemegol yn gymharol sefydlog, gyda gwrthiant tymheredd uchel da, ymwrthedd tymheredd isel, ymwrthedd i asid cryf, alcali cryf ac ardderchog arall. priodweddau.
Gellir defnyddio gwifren syth titaniwm ar gyfer weldio offer titaniwm, rhannau titaniwm yn prosesu deunyddiau crai, a ddefnyddir yn gyffredinol mewn dwy agwedd, mae un fel rhan strwythurol i brosesu cynhyrchu rhannau safonol ymhellach, rhannau strwythurol offeryn manwl, tlws crog, sgrin, ac ati; Yn ail, nifer fawr o offer titaniwm, awyrofod a llongau gofod, cynhyrchion milwrol, proses weithgynhyrchu deunydd ysgrifennu o weldio; Y trydydd yw'r wifren uwch-ddirwy a ddefnyddir yn uniongyrchol mewn rhannau offer rheoli ar gyfer rhannau strwythurol offeryn manwl. Mae gan y tri defnydd uchod ofynion uwch ar manwl gywirdeb ac ansawdd wyneb gwifren titaniwm.